I like to experiment with combining products. Anyone ever combine DG 501 and Megs 205 on a white polishing pad? Just curious how well these would work together. Should I even attempt this combo? Maybe at 2 dots each per panel.

Thoughts?
 
I like to experiment with combining products. Anyone ever combine DG 501 and Megs 205 on a white polishing pad? Just curious how well these would work together. Should I even attempt this combo? Maybe at 2 dots each per panel.

Thoughts?


I have read of mixing Mernz 106ff or SIP. You may want to use matching abrasive. 501 is DAT where 205 is SMAT. The mernz products are DAT
 
I used a 1:1 mix of m105/d300 with mf cutting pad and did some serious correction in 2-3 passes and it finished lsp ready.
 
If you're looking for more cut just go with Duragloss #671 Swirl Mark Remover.
 