redboost10
New member
- Feb 1, 2009
- 382
- 0
So i started with menz nano/super finish with a grey pad on the quarter panel and it got the swirls out, but it also left some new scratches or marring. You can see the before and after pictures. Before I go any further, I wanted to get your guys' opinions. I think I may have put too much water on the pad to start with...maybe too much polish? any help is appreciated. Thanks guys. should i stick with the grey pad? i went left/right and up/down 4 times in this area, moving about 1"/1 sec. but when i lifted up after polishing, i had a spot (which you could see) that was like the pad was too wet or too much polish?
1st picture is before
2nd picture is the amount of polish i used
3rd picture is right before removing the polish
4th picture is after
1st picture is before
2nd picture is the amount of polish i used
3rd picture is right before removing the polish
4th picture is after