rotzilla
New member
- Sep 28, 2011
- 79
- 0
Brief history;
I had a 09 ram, every time it would come in contact with road de-icer it would develop tiny rust spots on the chrome/stainless steel (plastic and metal) almost immediately, left unwashed would it would etch into the plastic. At the time I was using a meg's nxt.
Then I had a 11 ram, due to warranty issues the truck never had a layer of wax on it until just before I traded it in, however when it came in contact with the de-icer it never rusted. I thought the manufacturer had rectified the problem.
Now I have a 13 ram that came in contact with magnesium cholride for the first time last week, a few days later and rust spots are developing everywhere there is chrome and stainless steel. The truck had 2 recent coats of collinite 845. I used chrome polish to remove the rust and reapplied 845.
So the question is, is anybody else having similar issues, and what are you using or can be done to prevent further outbreaks.
I had a 09 ram, every time it would come in contact with road de-icer it would develop tiny rust spots on the chrome/stainless steel (plastic and metal) almost immediately, left unwashed would it would etch into the plastic. At the time I was using a meg's nxt.
Then I had a 11 ram, due to warranty issues the truck never had a layer of wax on it until just before I traded it in, however when it came in contact with the de-icer it never rusted. I thought the manufacturer had rectified the problem.
Now I have a 13 ram that came in contact with magnesium cholride for the first time last week, a few days later and rust spots are developing everywhere there is chrome and stainless steel. The truck had 2 recent coats of collinite 845. I used chrome polish to remove the rust and reapplied 845.
So the question is, is anybody else having similar issues, and what are you using or can be done to prevent further outbreaks.