I'm looking at Menzerna SF4000 or Megs M205 as a polish to remove some light swirls and water spots using a PC. How do these two polishes compare in terms of ease of use, correcting ability and gloss?
Thanks!
They should be about the same finish quality wise.
M205 should have more correcting ability if needed with the SMAT technology using a more aggressive pad if needed and it's very easy to work with and remove. Buffing times are pretty long as it doesn't flash very easy.
Both should give that great wet look after polishing though.
I would say try both as you really can't lose either way.
How difficult is the Menzerna to remove? I had some Final Polish many years ago, and it was very unforgiving as to the window to stop working. Just a moment too soon and it was a sticky mess, and a moment too long and it was like cement.
Make sure you prime well and apply thin. With a DAT product like Menzerna, its essential to break it down properly before buffing off. SMAT products like Meguiars require 2-3 passes and your done. Both work very well if used correctly.
Are these two products roughly equivalent in correcting level?THIS!:iagree:
The C6 has what you'd normally call 'hard' paint. That means 205 will likely finish down better than say if it were Toyota 'soft' black.
Working with 205 you do 3 maybe 4 section passes and wipe the product off BEFORE it dries. If you need more 'finishing' you reload the pad with 2~3 dime sized drops and do it again, 3 no more than 4 more passes.
Working with Menzerna you'd do 4 or so section passes with a machine speed of say 4.5 or so (on the PC machine) with medium arm pressure. Then a VERY light spritz, more like a fine fine mist with distilled water on the pad (or panel, just don't get it too wet), turn the speed up to 5.5-ish and lower your arm pressure then do a couple more section passes. Watching for the product to work down to almost nothing and it'll wipe away really easily.
Too much product and it'll gum up, too little and you'll dry buff. Especially with SMAT products like 205. FWIW, I'd do it with 205 because it'll do it faster and easier. Now if you want to jewel it down even more afterwards, Menzerna. :xyxthumbs:
Are these two products roughly equivalent in correcting level?
Are these two products roughly equivalent in correcting level?
No, not at all!
M205 will cut better throughout the working cycle. Where SF4000 will finish better, AFTER it's been broken down. (see below)
SF4000 imho wouldn't cut near as good, not even with the first pass (before it starts to break down). Although DAT products (if they were both starting as the same cut level of product) do tend to cut better right there, first pass, then they start breaking down.
This however is what makes them finish better.
I'd say to get one that has similar cut and finish to 205 you'd look more at IP2000, or MAYBE, just maybe PF2500. They are more of the 'polishing' compounds rather than 'finishing' compounds.
It appears that M205 is not really a finishing polish as the name implies, at least in comparison to the Menzerna products. I went ahead and purchased both. I'll start with the SF4000, and if not strong enough I'll use the M205 and then go back to the SF4000 if necessary.c7424:
I know it varies given a multitude of conditions, but how long can M205 be worked on average at about 75 degF for a 2'x2' section? I found some recommendations on a web search that says 20-30 seconds in 2-3 passes, but some Youtube videos show working it much longer on the order of 75-100 seconds with 6-8 passes.