ASPHALT ROCKET, What would be the reason not to use a Q/D to prime pads. What do you know that I don't know. Could you please share??? Thank you!!!
Doesnt FK425 and ONR contain polymers?They contain silicones which should not be mixed with your polishes. All you need is the polish itself to prime the pad.
The principle behind priming your pad is so you're not dry buffing your finish with the section of the pad that doesn't yet have product on it. It's not a big deal to do this if you work into the bead of your product properly and disperse it evenly across the face of your pad. Or, like some prefer to do, you can also add the product directly onto your pad. Another option is to spritz some water on the polished surface or on the pad itself to lubricate too.
:iagree:, also the you do not want to induce any other type of product into your product then it does not work as well. I have played around with this for a long time and the QD does cause a problem, so the safe way to prime a pad is use the product itself or if you feel better about putting something on the pad before starting just spritz it with water.
Hey its a learning curve. Being stupid is not asking questions and doing the wrong thing over and over.