why is it so hard to take i work it in for like 5 seconds and it drys up?
 
Well i start using that also will tonight but on a white Kompressor foam pad.Maybe your not using enough product or the pad is too dry .I think with a new pad you need some extra product on it untill it has absorb some Megs
 
i found it to be dry also. i followed the instructions with my udm and used the slow hand technique but i couldn't get much more than 1 pass before the polish was done. perhaps a spritz of water would help?
 
don't put the 105 on the pad, squirt a 2-3 inch line on the paint and pick it up as you slide the pad across that linesquezzing the trigger. do it at the angle so that it works right into the pad and paint without splattering. it does dry up quick and it will get dusty..even if you're spritzing QD. the stuff has a lot of cut but it finishes down like a medium polish.
 
M105 flashes quickly, you need to use a little more than usual.
if using a wool pad pick the polish up of of the car, with foam apply it to the pad, once you are going to use alittle more than Menzerna. With the foam pad it will work a little longer.
 
i found it to be dry also. i followed the instructions with my udm and used the slow hand technique but i couldn't get much more than 1 pass before the polish was done. perhaps a spritz of water would help?
Spray bottle with purified water works the best.been there and done that.
 
Well i start using that also will tonight but on a white Kompressor foam pad.Maybe your not using enough product or the pad is too dry .I think with a new pad you need some extra product on it untill it has absorb some Megs

I wonder were you learned that. That is an awesome combo.
 
I wonder were you learned that. That is an awesome combo.
I spoke to Jamores on the phone earlier .I think i got him on the right track (Wonder who told me ) After a good two hours i think i have my combo down .Will hit it again in the morning
 
I spoke to Jamores on the phone earlier .I think i got him on the right track (Wonder who told me ) After a good two hours i think i have my combo down .Will hit it again in the morning

Man, looks like I wont be sharing anymore secrets with you:D
 
Hey asphalt thats not nice lol. Were suppose to share secrets here! :righton: but yeah im stressing over my m3 because It isn't coming out the way I want it to. Harley you told me go straight from 105/pfw/ to sip/white to nano/ blue?
 
Hey asphalt thats not nice lol. Were suppose to share secrets here! :righton: but yeah im stressing over my m3 because It isn't coming out the way I want it to. Harley you told me go straight from 105/pfw/ to sip/white to nano/ blue?
I used ultrafina on a blue pad . White SIP then blue pad .I guess if you dont have the ultrafina use nano
 
:( Im going over the scratches and they dont budge !!! I used sip and white and there still there!
 
:( Im going over the scratches and they dont budge !!! I used sip and white and there still there!
If you used the wool pad and they are still there at this point i would do what you can.Wait untill DF i'm sure there will be plenty of guys there to help sort this out for you.Rather you wait then risk burning the paint.My came alot better with the M105 and Sip but there are still some spots on it .
 
Ok so I did a panel with m150 pfw sip on white and nano on blue the nano blue step removed EVERYTHING! i guess the nano step was the most important lol
 
Ok so I did a panel with m150 pfw sip on white and nano on blue the nano blue step removed EVERYTHING! i guess the nano step was the most important lol
Yes for sure the wool and white will leave there own swirls or marring .If you really want to go crazy use ultrafina or 85rd .Ultrafina you can pick up local 3m product
 