I've read on some forums that several have found postive results by mixing AW and FC&S. Just bought a gallon of each (actually the marine FC&S) and thought it might be worth a try--cleaning ability, slickness and sealant.

Anyone try it here and does the theory seem worthy? 50/50 looks like the popular mixture. Only worry is using AW too often as many warn that it can mute the paint--especially metallic flakes.

Always experimenting and asking...
 
I use a mix of 70/30...70 FC&S and 30 AW....its sorta a cleaner QD with Umpf...that was my best mixture...no build up....

I have not mixed it with the marine yet...since the Marine has more UV protection in it...I did not want to Dilute it...\

AL
 
Hmm...wondering if an 80/20 or 90/10 mix with the 521/AW might work?

Guess I'm never satisfied with stock solutions. :)
 
Al-53 said:
I use a mix of 70/30...70 FC&S and 30 AW....its sorta a cleaner QD with Umpf...that was my best mixture...no build up....

I have not mixed it with the marine yet...since the Marine has more UV protection in it...I did not want to Dilute it...\

AL
:iagree: Then you can call it DG#1872 or #1472!:D
 