What can cause very fine micromarring/buffer trails?

purplenurple

New member
Joined
Jun 4, 2007
Messages
144
Reaction score
0
Last month I decided to polish a fender on my GTO to test out the PC, and got some micromarring. I was using the PC with a white pad w/1Z High gloss polish on speed 5-6. I really dont know what could have caused the very, very, very fine swirls that were only visible in direct sunlight. Maybe I was trying to work too big of an area? Not enough product (quarter size blob, about 3 or 4 quarters tall)? Dry buffing? ONR QD on Pad? Too fast a speed for the soft-ish clear? Not working the polish in enough? (usually did one pass on 5-6 and then the polish would be almost completely dry and then a pass at 3-4.

Thanks for any suggestions...
 
some polishes just dont finish down well enough on there own. Thus the need for a lighter finishing polish and lighter pad. It sounds like this could be your culprit.
 
Ok, thanks guys.
Killr - The White pad and the high-gloss polish are as light as anything. Maybe I wasnt using enough pressure....

How do you guys wash your pads, BTW? I just use an old toothbrush and dawn...
 
Ok, thanks guys.
Killr - The White pad and the high-gloss polish are as light as anything. Maybe I wasnt using enough pressure....

How do you guys wash your pads, BTW? I just use an old toothbrush and dawn...
Try Dawn Power Dissolver.
 
Try priming the pad with a few sprays of Distilled water before putting the polish on it. Sometimes a few sprays are needed on the pad once the polish has been worked a little bit to extend the working time of the polish.
 
dry buff, dirty pad, polish not breaking down

all of these i thought of when reading the post and all were answered!

haha i guess its process of elimination now, huh? :)

new finishing polish: Menz 106ff = <3
 