K
Kappy
Guest
Microswirls or rather scratches caused by m205.
The paint is so soft that even m205 on a white pad leaves it's own marks.
My process was M205 on orange followed by m205 on red. That led to really good results.
Thanks for the info.
I think that this might be the first I've read about using the same polish on two different pads; one to remove the defects and the other to finish the job. Apparently there are many different methods that can produce a good result, if you have the tools to try them.
When I bought my DA I ordered some of the orange and white LC flat pads, and then at the last minute decided to order one of each color of the LC Hydro-Tech pads, which included a red one. Is that the type of red pad you used?