Hi All,
I have a paint gauge and the paint is all reading around 80um so i do not want to do risk clear coat failure by correcting the paint. What specific products do you all recommend that will help fill the marring/wash induced swirls? And will last more than a wash or two? If its a glaze ideally it can be topped by a sealant Duragloss TPP, WG3.0 without affecting durability.
Also what are your typically paint thickness readings for the cars you are correcting, what numbers give you pause?
Thanks!
I have a paint gauge and the paint is all reading around 80um so i do not want to do risk clear coat failure by correcting the paint. What specific products do you all recommend that will help fill the marring/wash induced swirls? And will last more than a wash or two? If its a glaze ideally it can be topped by a sealant Duragloss TPP, WG3.0 without affecting durability.
Also what are your typically paint thickness readings for the cars you are correcting, what numbers give you pause?
Thanks!