Are you guys using the optimum compound/polish with a DA? What pads are you guys having success with.
I have only used Opti Hyper compound and polish on the Opti MF cutting and MF polishing pads to date on my Flex DA.
I am late to the Opti Hyper product line, so the new MF pads were out by time I got here. Have yet to try them on foam, don't know if I would with the luck I have with defect removal on MF pad ( cutting or polish depending on the defect ).
The Opti MF cutting pad and Opti Hyper Compound I don't think would require the use of the Flex, so any DA ( PC, GG, Megs ) should be able to get the same results as the flex with this pairing.
The conversations I have had with others ( more knowledgeable than myself ) on the SIP / Opti Hyper Compound / M105 comparison put M105 as the best out of the 3 for very serious defect removal with a DA.
I am a shade tree detailer, so I don't think I would encounter any
requirement for using M105, but I do have the 8 oz sample bottles of M105/M205 in my cabinet just in case. I have yet to open them. So, I have all 3 major defect removal products, just in case...
I would hate to see what would need to happen to paint for me not to be able to correct it with Opti MF cutting and Hyper compound. Really wish I had gone Opti Hyper line before going Menz, think I would have passed on SIP / 106 combo. I don't think I could live without PO85RD now, I'm addicted to it.