Dana
How long should a section pass take with 105 on a 18x18 section? With wool... and with a pad... I can get 2 passes before dusting or 1 if i give some pressure and slow down to work on a RIDS and I think i confuse the dusting with drying... and I also figured out i was not using enough product... worked it to long... and let the pad cake up a few times on me...
I tried redoing it all spurring after each section and think I did a better job... Definitely think more procedure was a key to fixing defects within the short working time.
I ran outta 105 (damn 8 oz bottle that was more then 1/2 empty) before I got to practice with the white CCS and the 105 to see if i could remove halograms I put in with the wool.
Mulitple 205 + White CCS passes would not touch my marring though from the wool. Out of frustratin i grabbed the PCXP and Syn1 (from pb's beta test) and an org pad and with tons of pressure and multiple passes... This stuff did not do a single thing but put on a dust show! So the truck sits with ugly halograms on the side of the bed until my new pads backign plate and 32oz bottles of 105 and 205 come in... I will also test out Opt spray compound to see if it cleans any of it up.
I think for us newbies the short working time doesnt help when we make and extra pass outta unconfident decision making.
Anyway ill keep ya post and thanks for the hours of help Dana. Waiting for you to start making videos
Chris